Long-Term Part Design
Creep in plastic parts is slow deformation under a load that never goes away. A clip, a shelf, or a boss can pass every test on day one and still sag, loosen, or crack years later. The data sheet modulus will not warn you. That number comes from a test lasting seconds. Your part lives under load for years. Design for the load over time, not the load in the test lab.
A part can pass today and still fail in a year
Plastic is viscoelastic. It springs back like a solid and flows like a very slow liquid. Load it and it moves at once. Keep the load on and it keeps moving. The first movement is elastic. The movement that follows is creep. Some of it recovers when you unload the part. Some of it stays.
Heat speeds the whole process up. A part that holds shape in a cool warehouse can sag in a warm cabinet. Stress does the same. Double the stress and the creep rate rises far more than double. That is why a small overload matters more than buyers expect. A bracket rated with room to spare at room temperature can still creep badly near a heater.
I have seen a wall-mounted housing pass a pull test, ship, and return a year later with its screws loose. Nothing had broken. The bosses had relaxed around the screws, a fraction of a millimetre at a time. The fix was not a stronger screw. The fix was less sustained stress on the boss.
Creep is not stress relaxation
Creep holds the load steady and watches the shape change. Stress relaxation holds the shape steady and watches the load fall away.
Creep and stress relaxation come from the same material behaviour. The test conditions differ, and buyers mix them up. A bolted plastic joint lives in the second case. The plastic keeps its clamped length while the clamping force bleeds off.
Both matter in one assembly more often than people admit. A cover screwed down tight relaxes. Its clamping force drops. Then vibration or a bump finishes what relaxation started. If your joint must stay tight for years, do not rely on the plastic alone to hold the clamp load. A metal insert, a spring washer, or a through-bolt with a nut carries that job better. Each adds cost or assembly time. A loose cover in the field costs more.
Read the creep modulus, not the data sheet modulus
The modulus on a data sheet is a short-term number. Creep modulus is the same idea measured after a stated time under load at a stated temperature. It falls as time passes. Use it in deflection checks for any part that carries load for weeks or longer. Use the short-term modulus only for brief loads, like a snap during assembly.
Ask your resin supplier for isochronous stress-strain curves for the exact grade you plan to buy. Each curve shows strain at one elapsed time across several stress levels. Read the strain at your service life, not at 1,000 hours, unless your part retires that early. Curves from tests run to 1,000 hours are often extrapolated to about 100,000 hours, roughly 11 years, under ASTM D2990. Extrapolation is a prediction, not a guarantee. Treat it as one, and keep margin in the design.
When no curve exists for your grade, do not borrow numbers from a similar grade and call the job done. Test the real grade, or pick a grade with published long-term data. Similar grades differ in filler, molecular weight, and processing history. Those differences move creep behaviour more than a data sheet suggests.
As an illustration of how much material choice matters — from one trade source, Dr Charlie Geddes (Interplas Insights, 2014), not a grade-specific test result: after one year at room temperature under a modest 5 MPa load, polypropylene showed about 1.5% creep strain, against about 0.2% for polycarbonate under the same conditions; at 60 °C the polypropylene figure rose to about 2.5%. The same source describes polyacetal (POM), because of its higher crystallinity, as about five times more resistant to creep than polypropylene — a qualitative comparison, not a measured strain ratio. Treat these figures only as an illustration of the differences between material families; for any real part, use the resin supplier’s creep data for the actual grade, temperature, stress and design life.
Where creep in plastic parts shows up first
Creep finds the highest sustained stress first. Bosses under screw load head the list. A boss holds a screw. The screw holds the clamp. The plastic between them carries the load for the life of the product. Thin walls near a load point come next. So do cantilever clips left in a bent position, shelves under constant weight, and snap arms that stay deflected after assembly.
Gate position can make the problem worse. Melt flow aligns polymer chains and glass fibres along the flow direction. A load pulling across that direction meets weaker, faster-creeping material. Weld lines in a loaded area behave the same way. They are already the weak line in the part. Sustained load opens them slowly. Keep weld lines out of load paths where you can. When you cannot, lower the stress there and prove the joint with a long test.
Watch for creep in places that look unloaded. A part clipped into a housing may sit under a small permanent bend. That bend is a load. Months later the clip loses grip. The part still looks fine on the bench. It fails only because the grip force has gone. Design clips to rest unloaded, or accept that the holding force will fall and size the clip for the fallen value.
Lower the stress before you change the resin
The cheapest fix for creep in plastic parts is usually geometry, not a dearer resin. Lower the stress and creep slows sharply. Spread the load over more area. Add a rib, but place it where it carries load instead of where it looks tidy. A rib that only thickens a wall can raise local stress at its base. Give rib bases a generous radius. Keep rib thickness in line with the wall thickness guidance in our wall thickness masterclass. A well-sized rib stiffens the part without leaving a sink.
Choose the resin for the service life, not the catalogue headline. Glass fibre reinforcement slows creep because fibres restrain chain movement. It also raises stiffness and warpage risk, and it wears steel faster. Crystalline resins such as polyacetal generally creep less than polypropylene, but they shrink more and need tighter process control. Amorphous resins such as polycarbonate creep less still in the comparison above, yet they cost more and scratch more easily. Pick one option for the common case: a glass-filled grade of a resin you already mould well. It must have long-term data at your service temperature. Prove it with a loaded test at temperature, not with a room-temperature pull test.
Use a metal insert or a through-bolt where the load is real. Use the boss design for self-tapping screws only where the load is light and short-lived. Inserts add a step and a part cost. They repay that cost the first time a cover stays tight.
Set a strain limit before you run numbers. Decide how much permanent movement the function allows. A shelf that sags 2 mm may still work. A seal face that moves 0.2 mm may leak. Work back from that limit, through the creep modulus at service life and temperature, to the stress you can allow. Then check the design against that stress with a safety factor of at least 2.0 on the long-term limit. Use a higher factor where failure hurts. If the numbers do not close, change the geometry or the resin before cutting steel. Steel changes after T0 cost time, money, and credibility.
Frequently asked questions
How fast does creep happen in a plastic part?
Creep starts the moment load is applied and continues for as long as the load stays. The rate is fastest early, then slows, but it does not stop on its own. Heat and higher stress both speed it up. A part that looks stable after a week can still move measurably after a year.
Can creep be reversed by unloading the part?
Part of the deformation recovers when the load is removed. The elastic part springs back at once. The viscoelastic part recovers slowly. The viscous part does not recover at all. After long service under load, expect some permanent set. Do not promise a customer that a sagged part will return to shape.
Which plastics resist creep best?
No single resin wins in every case. Glass-filled grades creep less than unfilled grades of the same resin. Crystalline resins such as polyacetal generally creep less than polypropylene. Polycarbonate creeps less than polypropylene in published comparisons. Choose from long-term data for your exact grade, temperature, and stress. Catalogue strength alone is a poor guide.
Does creep affect snap fits and clips?
Yes, and clips are a common failure. A clip held in a bent position relaxes, so its holding force falls over time. Design clips to sit unloaded at rest where possible. Where a clip must stay deflected, size it for the relaxed force, not the fresh force. Test the clip after ageing under load at service temperature.
How do I test for creep without waiting years?
Run loaded tests to at least 1,000 hours under ASTM D2990, at several stress levels and at service temperature. Plot the results and extrapolate with care. Time-temperature superposition can shorten testing, but it needs care near the glass transition temperature. Always confirm a critical design with a real part under real load.
Will a thicker wall stop creep?
A thicker wall lowers stress, so it slows creep. It does not stop creep. Thick sections also cool slowly, shrink more, and risk sink marks and warpage. A ribbed wall usually beats a thick solid wall. Spread the load, keep walls even, and check the result with creep modulus at service life.
What load will this part still carry in five years, at the hottest temperature it will see? Answer that question with data for the exact grade, and the rest of the design follows.