Fastening & Assembly
Threaded inserts put the thread in metal and the load into a much larger area of plastic. A molded thread in the plastic itself works only where a joint is made once and never serviced. Heat staking removes the thread altogether and locks the mating part in place for good. So the choice turns on service. Does this joint ever need to come apart again?
“Heat Staking” Means Two Different Things
The trade uses one phrase for two different jobs, and the confusion costs buyers real money. In the first job, a heated brass insert is pressed into a molded hole. The melt flows into the knurls and undercuts, then freezes around them. The part keeps a metal thread. In the second job, a molded plastic boss is heated and re-formed into a rivet-like head. The head clamps a circuit board, a shield, or a bracket in place. No thread remains.
Heat-set installation puts a thread in. Heat staking takes the thread away. The service question decides which one fits.
Heat staking leaves a thread behind only when the heated part is a brass insert. When the heated part is the plastic boss itself, no thread remains. Ultrasonic staking works the same way as the second job. The heat comes from vibration at about 20 kHz, not from a heated tool. Keep the two meanings apart and the rest of the decision gets simple.
Why a Plastic Thread Gives Up First
A thread cut or formed directly in plastic has a small shear area, and plastic under sustained clamp load creeps. The clamp force present on day one is gone months later. Each disassembly wears the thread a little more. A housing screw that felt tight at first assembly can spin freely after the third service visit. That is the failure buyers describe most: not a broken part, but a joint that no longer holds.
A threaded insert changes the load path. The screw bites into brass, and the brass spreads the load across a much larger plastic area through its knurls. The insert itself does not creep, so the thread stays put while the joint is undone and redone. The plastic around the insert can still creep, crack, or pull out if the boss is wrong. An insert is not a repair for a bad boss. It is a thread that survives service, nothing more.
Which Threaded Insert Fits Your Joint
Five options cover nearly every joint, and the service question picks among them. A self-tapping screw into a boss is the baseline for housings assembled a few times at modest torque. Our guide to boss design for self-tapping screws covers that baseline in full. When the joint must be undone repeatedly, take real torque, or hold clamp load over time, move to a post-mold threaded insert.
| Option | Use it when | What it costs you |
|---|---|---|
| Molded thread in the plastic | Assembled once, lightly loaded, never serviced | Weakest joint, no extra part |
| Self-tapping screw in a boss | Assembled a few times, modest torque | Fails on repeated service or sustained load |
| Heat-set insert | Repeated disassembly, real torque, clamp load over time | A secondary operation and a bought part |
| Ultrasonic insert | High volume, small features, tight cycle time | Horn and fixture setup, more tuning |
| Molded-in insert | Highest pull-out demand, or no access after molding | Cycle time, handling, scrap on a misplaced insert |
| Press-in or expansion insert | Non-critical joint, ease of install matters most | Lowest torque and pull-out performance |
Heat-set inserts are the default post-mold choice. Plastics Technology calls them the best mix of performance and installed cost among post-mold options. The insert is heated and pressed into a slightly undersized hole, and the melt locks into the knurls as it cools. One rule governs the operation: let the joint cool undisturbed. Moving or loading the part before the melt has set shears the bond. Ultrasonic insertion does the same job faster, in fractions of a second, and suits small features and high volumes. It needs a tuned horn, a rigid fixture, and a supported part. Thin or poorly supported walls can crack if the setup is rushed.
A molded-in insert gives the highest pull-out and torque of all. It also costs the most in practice. Every shot pays for loading and handling, and a displaced insert scraps the part. Use it where the load or the access justifies that cost, not as the default. A self-tapping insert cuts its own thread as it is driven in, and one guide rates its pull-out best among post-mold inserts. The installer must keep it square to the hole. A tilted insert will not mate with the screw. Press-in and expansion inserts are the cheapest to install and the weakest in service. Treat them as a choice for non-critical joints, not as an equal to heat-set.
The Boss Decides the Joint, Not the Brass
A failed insert joint is usually a boss or hole failure, not a brass failure. The insert was in tolerance. The boss was too small, the hole was oversize, or the setting temperature was wrong. Four numbers decide the joint, and all four belong on the drawing. Size the boss outer diameter at about twice the insert outer diameter. That gives the plastic around the insert enough material to carry the load. Take the hole size from the insert maker’s specification for the actual resin, never from a guess. Glass-filled resins need different holes than unfilled ones, and the maker publishes both. Make the hole deeper than the insert so displaced plastic has somewhere to go — and deeper than the screw will ever reach, or a bottomed-out screw jacks the insert out of the boss. SPIROL’s rule is insert length plus two thread pitches, so the extra depth grows with thread size, about 1 mm on an M3 and 2 mm on an M6, and a second guide puts the typical extra depth at 1.5–2.5 mm. There is no single millimetre figure: take the depth from the insert maker’s specification for that insert and resin. Keep the boss wall at 0.5 to 0.6 times the nominal wall where it meets the part wall. A thicker boss wall sinks the show face. Our wall thickness masterclass explains why that ratio matters.
A stable, documented process keeps molded-in inserts in the same place shot after shot. That consistency matters more once inserts go into the mold. Brass is the common insert metal. Steel inserts fit the same boss where torque, wear, or a structural joint needs more than brass. A structural or safety joint normally moves to a steel insert with a larger boss, or to metal-to-metal fastening entirely.
Heat Staking: When the Joint Never Comes Apart
Heat staking suits the joint that never needs to come apart. A printed circuit board, a metal shield, a label plate, or a bracket is set over a molded post. The post is heated and re-formed into a head that captures it. No fastener is bought, lost, or over-torqued. No thread can strip. The trade is permanence. A staked joint cannot be taken apart without destroying the head, so the decision is permanent. Size the formed head to cover the mating part’s hole with margin. Branson’s staking guide makes the head diameter depend on the profile: 1.5 times the post diameter for a low-profile dome stake, 2 times for a high-profile dome, rosette, hollow or knurled stake, and 1.9 times for a flush stake — so 1.5× is one profile’s figure, not a general rule. As a cross-check, one equipment guide sizes the head so it overlaps the mating hole by at least 1.5 mm per side. Take the head dimensions from the staking-equipment guidance for the actual post profile and mating part. Keep the boss wall at roughly half to two-thirds of the surrounding nominal wall so it cools evenly and does not sink. The tool must hold the head while it cools and re-solidifies. Pulling heat and pressure early leaves a weak, distorted head. Support the mating part under the post during staking, or the part flexes and the head forms crooked.
Heat staking suits large bosses and awkward shapes. Ultrasonic staking suits small posts, closely spaced features, and assemblies with heat-sensitive electronics nearby. Cycle times run shorter, and no hot tool needs cooling between strokes. Staking adds a secondary operation and fixture cost that a snap-fit or a screw may avoid. It also needs the post in the mold design from the start. A post added late means a mold change.
What to Ask Your Supplier Before You Approve the Joint
A catalogue pull-out figure measured in one resin at one boss size is not your part’s pull-out figure. Ask for the insert maker and part number, the boss and hole drawing with tolerances, and the installation method with its settings. Temperature, pressure, and hold or cool time all belong in the record. Ask for pull-out and torque results on your exact resin and boss, sampled per lot. The 9 proven DFM rules cover the wall transitions and stress concentration where a boss meets the wall. Those rules decide whether the boss survives the insert. For a staked joint, ask for the formed-head dimensions and the cooling and hold step in the staking cycle. Also ask for a cross-section or destructive sample from first production.
Frequently Asked Questions
Can threaded inserts be used in any plastic?
Heat-set and ultrasonic inserts suit thermoplastics, which soften and re-freeze. Thermosets do not re-melt once cured, so heat and ultrasonic installation cannot be used on them. Self-tapping, press-in, and expansion inserts are the options for thermosets. The resin and the installation method must be chosen together, not separately.
How many times can a threaded insert be assembled and disassembled?
The metal thread itself survives hundreds of assembly cycles without degrading, which is the point of the insert. The limit is usually the boss around it, the screw, or the torque applied at assembly. A joint that must be serviced often still needs a torque specification and a boss sized for repeated loading.
Is a molded-in insert stronger than a heat-set insert?
Yes, molded-in inserts give the highest pull-out and torque performance, because molten resin flows under pressure into deep undercuts. The cost is cycle time, handling, fixturing, and scrap when an insert is displaced. Reserve molded-in inserts for the highest loads or for spots no post-mold tool can reach.
What is the difference between heat staking and ultrasonic staking?
Both re-form a plastic boss into a head that captures another part. Heat staking warms the boss with a heated tool, which suits large bosses, glass-filled resins, and vibration-sensitive assemblies. Ultrasonic staking generates heat by friction at about 20 kHz, which suits small posts, tight spacing, and heat-sensitive electronics nearby.
Can a heat-staked joint be taken apart for repair?
No. Disassembly destroys the formed head, and the joint cannot be re-staked. If the assembly may need service, choose a threaded insert or a screw instead of staking. Staking is the right answer only where the joint is permanent by design.
How do I specify a threaded insert on a drawing?
Name the insert maker and part number, the hole size and tolerance, the boss outer diameter, and the hole depth. Add the installation method and its settings, and the pull-out and torque test evidence for the exact resin and boss. A drawing that lists only the thread size has not specified the joint.
A supplier who cannot name the insert maker, the hole tolerance, or the test behind the number has not designed the joint. Before you approve the drawing, ask which part of this joint carries the load at the tenth tightening.