Material Selection
Most parts take 10–30% regrind in injection molding without losing the properties that matter. Regrind is ground-up sprue, runner, and rejected parts blended back into virgin resin. The safe number depends on the resin, the part, and how the regrind was handled. No supplier can quote one percentage without asking what the part must do.
Regrind Is Not One Material
Buyers hear one word, regrind, and picture one material. The floor sees three streams, and they behave nothing alike. In-house runner regrind is the cleanest of the three. It comes from the sprue, runner, and gates of the same job, in the same grade and the same color. Its heat history is a single pass through the barrel.
In-house rejects and trim sit one step down. They share the grade, but they passed through handling, labels, or a bad shot first. They are still traceable, and a careful shop can use them.
Bought reclaimed pellets sit at the far end. They come from post-industrial or post-consumer waste, ground outside your factory. Melt flow, color, and odor vary between batches. They cost the least per kilo and demand the most inspection.
In-house runner regrind is the same resin you already approved, ground up. Bought reclaimed pellets are a new material that happens to share a name.
Keep the streams in separate bins, one per resin and color. A single scoop of the wrong resin poisons a whole batch. A cold runner can be a fifth to half of the shot weight, so the stream is not small. That scrap is the material at stake.
Why Regrind in Injection Molding Loses Strength First
A part passes its dimensional check and fails in the field. That is the classic regrind failure, and it has a plain cause. Each heat cycle shortens the polymer chains. As the chains shorten, melt viscosity, impact strength, and elongation fall with them.
Regrind leaves stiffness mostly alone and attacks impact strength instead.
Stiffness usually holds up, so the part still feels solid. Impact strength and elongation go first, and the part turns brittle where it bends, snaps, or takes a hit.
Weld lines suffer more than the bulk material does. Regrind lowers the strength of a weld line faster than it lowers the rest of the part. Put a structural boss on a weld line and the failure finds it first.
Glass fiber adds a second kind of damage. Fibers break at every pass through the grinder and the barrel. Stiffness and warpage shift even when the part looks fine.
Heat history adds up. The same batch, reground again and again, degrades a little more each time. Retire old regrind to a less demanding part, or throw it away. Recycling it forever is not a plan.
Safe Regrind Ratios by Resin
There is no universal percentage, and any supplier who quotes one without asking about the part is guessing. The table below gives working ceilings we use as starting points for a test. They are not numbers to quote on a drawing.
| Resin | Working ceiling (share of total shot) | Watch first |
|---|---|---|
| PP, PE | 20–30% | Color drift, odor |
| ABS | 15–20% | Impact strength, gloss on texture |
| PC | 15–20% | Yellowing, drying |
| PC/ABS | 15% | Weld-line strength at bosses |
| PA6, PA66 | 15–20% | Moisture pickup, drying |
| POM | 10–15% | Yellowing, odor |
| Glass-filled grades | 10–15% | Fiber breakage, warpage shift |
| Food, medical, optical | 0% | Validation rules regrind out |
Those percentages are a share of the total shot, not of the virgin share. At 20% regrind, one part in five is ground material. Dose it by weight, or with a feeder that is actually calibrated. Never by eye into the hopper.
For a common case, start at 15%. A general industrial PP or ABS part with no cosmetic face is the common case. Test it, and step up to 20–25% only if the tests pass. A ratio that works on a thick housing can fail on a thin snap arm in the same resin.
The grinder sets how much regrind you have. Your tests set how much you can use.
What Ruins a Regrind Batch
Regrind in injection molding fails most often at the grinder, the bin, or the dryer.
Contamination kills a batch faster than heat history does. The wrong resin, the wrong color, a paper label, or metal from worn grinder blades all count. Magnetic separators catch metal, and a clean bin policy catches the rest. One contaminated bin can scrap a whole shift of parts.
Moisture is the second trap. Ground material has far more surface area than pellets, so it picks up water fast. Dry regrind again before use, to the same spec as virgin resin. Silver streaks on a PC part at 20% regrind usually mean wet material, not bad regrind.
Fines cause the black specks. The dust-sized fraction scorches at the screw and marks light parts. Screen fines out, and keep grinder blades sharp. A dull blade makes more fines and heats the material while it cuts.
Uneven granulate feeds unevenly. Shot-to-shot variation follows, and parts start failing dimensional checks. Keep granulate close to pellet size, and check the screen, not the habit.
Color drifts between batches, and masterbatch choice cannot fully hide it on a cosmetic face.
Most regrind failures come from handling, not chemistry. A dirty bin, a dull blade, or a wet batch does the damage.
How to Prove a Ratio Before You Ship It
Test the blend you will ship against a virgin baseline. Mold test bars at the target ratio, then check melt flow index, tensile strength, and Izod impact. Accept the blend only if the properties the part depends on stay inside your limit.
A mold validated on virgin resin and then run at 20% regrind was never validated at all.
Validate the blend at the trial. The mold trial checklist for T0 covers what to verify before you approve a mold for production.
Re-validate when the ratio changes, when the regrind source changes, or after a long stop. Label each bin with resin, color, date, and number of passes. When melt flow drifts far from the virgin baseline, downgrade the batch or discard it. That drift is the signal that the material has had enough heat.
Ask the supplier for the test data at the agreed ratio, in writing, before the order. If a supplier runs regrind without telling you, the first sign is usually a customer complaint.
When the Answer Is Zero
Food contact, medical, optical, and customer-specified parts usually rule regrind out. Traceability and validation decide, not cost. Most specs for those parts require virgin resin of an approved grade.
Tight tolerances are the next no. Regrind shifts shrinkage a little, and a little is enough to move a tight feature out of tolerance. A virgin validation run and a production run at 20% regrind are two different processes.
High-gloss, clear, and white parts follow the same rule. Color drift and specks show first on a cosmetic face.
Recycled-content targets add one more limit. European packaging rules count only post-consumer material, not production scrap. In-house runner regrind does not count toward those targets. If a buyer asks for recycled content, they usually mean bought PCR, a different purchase with its own price and inspection.
Ask what the part must survive, and whether anyone tested the blend at that ratio.
Frequently Asked Questions
How much regrind can I use in injection molding?
There is no universal percentage. Commodity PP and PE parts often run 20–30%, ABS and PC 15–20%, and glass-filled grades 10–15%. Treat those numbers as starting points, not specs. The safe ratio depends on the resin, the part, and how clean the regrind is. Test the exact blend you will ship before you commit to a number.
Does regrind weaken plastic parts?
Yes, but not evenly. Each heat cycle shortens polymer chains, so impact strength and elongation fall first while stiffness usually holds up. The part turns brittle rather than weak. Weld lines and snap fits suffer most. A part can pass a dimensional check and still fail a drop test. Test impact strength at the blend ratio you will ship.
Can regrind be used for food-contact or medical parts?
Usually not. Food-contact and medical parts need traceability and validation that mixed or reprocessed material rarely satisfies. Most customer specs for those parts require virgin resin of an approved grade. Ask the supplier for the material approval documents for the exact grade and color before you order. Treat any regrind proposal for a regulated part as a reason to pause.
Why do parts with regrind show black specks or silver streaks?
Black specks usually come from fines, the dust-sized fraction that scorches at the screw. Screen fines out and keep grinder blades sharp. Silver streaks usually mean moisture, since ground material picks up water faster than pellets. Dry regrind to the same spec as virgin resin. Both defects point at handling, not at the idea of regrind itself.
How do I test a regrind blend before production?
Mold test bars at the ratio you will ship and compare them with a virgin baseline. Check melt flow index, tensile strength, and Izod impact at minimum. Accept the blend only if the properties the part depends on stay inside your limit. Then validate the mold on that same blend. A ratio change or a new regrind source means the test runs again.