What to Measure Before Approving T1 Injection Mold Samples

Mass Production and Quality

What to Measure Before Approving T1 Injection Mold Samples

Measure T1 injection mold samples against the drawing, cavity by cavity, before you approve anything. T1 is the first trial that produces parts for measurement against the drawing. It shows whether the steel copied the approved design. It does not prove that the mold is ready for mass production. Most new molds need one or two rounds of correction after T1. Plan for that loop, and judge T1 by what it reveals.

Ask for a dimensional report for each cavity and parts bagged and marked by cavity. Ask for a process sheet that records plastic variables and a written list of open issues. Give every open issue an owner and a date. If any of these is missing, hold the approval until it arrives.

What Can T1 Injection Mold Samples Prove?

T1 proves whether the first steel cut matches the drawing, and it lists what still needs correction. T0 came first and checked that the mold fills, ejects, cools, and runs without damage. T1 is the first trial judged against dimensions, fit, function, and appearance. T2 follows and checks whether the corrections from T1 worked.

Trial Main purpose What you should receive What it does not prove
T0 Mold fills, ejects, runs, and cools Short shots and trial notes Dimensions or cosmetics
T1 First check against the drawing Dimensional report per cavity, process sheet, sample parts, and photos Stable production or final approval
T2 Corrections from T1 work Re-measured features and a change log Long-term stability across shifts

Treat a clean T1 as a good start, not as a pass. A part can measure well on one cavity and fail on the next. A part can look right and still carry a gate-seal problem that shows up later in cold weather. That is why the approval decision rests on records from every cavity, not on the best part in the box.

Agree the meaning of each trial with your supplier before steel is cut. Shops label trials in their own ways. A written scope for T1 stops arguments about what the samples were meant to prove. Our note on trial runs before production sets out the same sequence for preform molds.

How Do You Measure Each Cavity?

Measure every drawing dimension on parts from each cavity, and keep the results separate by cavity. An average across cavities hides the one cavity that runs out of tolerance. Mark each part or bag with its cavity number before measurement starts.

Start with the dimensions that decide fit and function. Mating faces, bore diameters, snap fits, seal surfaces, and hole positions come first. Cosmetic faces come later in the same report, not in a separate round of checks.

Measure parts from consecutive shots after the process settles. Hand-picked parts flatter the mold. A run of consecutive shots shows the spread your production will live with.

Record the datum and the instrument for each feature. A caliper reading and a CMM reading are not the same evidence. When a dimension sits near a limit, re-measure it on a second part from the same cavity. Do not call it a failure on one reading.

Compare each cavity against the same drawing revision. A report that mixes drawing revisions wastes the trial. Ask for the revision number on the report and on the samples.

Cavity spread often traces back to fill balance, and our guide to multi-cavity mold balancing shows how short shots expose it.

Check warpage on a surface plate with a feeler gauge, not by eye. A part that rocks on the bench will not seal in the assembly. Record the gap and the face it sits on, so the correction targets the right side of the steel.

What Does Part Weight Reveal?

Part weight reveals fill balance and gate seal that dimensions alone cannot show. Weigh parts from each cavity on the same scale, and record the weight beside the cavity number. A light cavity may be starved by its runner or gate. A heavy cavity may be overpacked. Both conditions can still pass a quick dimension check, and both will drift in production.

Ask for the gate-seal study with the T1 report. The study weighs parts at increasing hold times until the weight stops rising. That plateau marks gate freeze. Hold time past that point adds cycle time without adding part weight. John Bozzelli sets out the method in his guide to gate-seal experiments. The same weighing routine applies to your T1 parts.

Short shots add a second reading. A first-stage-only part should be visibly short, not full with sink. Compare the short shots cavity by cavity at the same shot size. Bozzelli puts first-stage fill at 90 to 99.9 percent by volume, not by weight. His note on first-stage fill by volume gives the reasoning.

Weigh the short shots when the visual difference is small. A few grams of spread across cavities in one shot is a balance reading, not a scale error.

How Do You Read the Process Sheet?

Read the process sheet for plastic variables, and treat machine settings as background only. A sheet that lists barrel zones and screw speed alone cannot transfer to another press. Fill time, melt temperature at the nozzle, transfer position, and gate seal time can.

Check the resin grade and lot on the sheet. Check the drying time and temperature for hygroscopic resins. A new lot or a damp resin moves dimensions without touching a machine setting.

Fill time deserves a close look. Once the fill time is set for a mold, it should stay close to that value through the life of the job. Bozzelli recommends holding it within 0.04 seconds of the set value. His article on evaluating fill times explains the viscosity curve behind that number and the limits of reading too much into it.

Ask for coolant flow per channel on a numbered watering diagram. A miswatered mold looks like a process problem until someone checks the hoses. Record mold temperature at the cavity surface, not on the controller screen.

A sheet built this way matches the scientific molding process window our shop documents for every job.

Compare the T1 sheet with the sheet you will use at production. If the press or the resin lot changes, the T1 numbers stop describing the job. A cooling change does the same. Note the change on the sheet, and date it.

How Do You Judge Fit, Function, and Cosmetics?

Judge fit and function on the assembled product, and judge cosmetics against the agreed surface standard for that face. Assemble the T1 part with its mating parts. Check clips, threads, seals, and fasteners under hand force first. A clip that needs a tool to close will fail on the line, even when its dimensions read well.

Look for sink where ribs and bosses meet the wall. Look for flash on the parting line, shut-offs, vents, and ejector marks. Look for weld lines where melt fronts met. Mark whether each line sits on a cosmetic face or in a stress zone.

Thick ribs and bosses pull sink into the opposite face. Our wall thickness ranges by material show the rib ratios that keep sink in check.

If texture is not yet etched, judge geometry first and leave the surface call for T2. Etching changes draft needs and hides small sink, so a texture decision made at T1 can mask a steel problem.

Photograph each defect with a scale ruler in the frame and a note of the cavity. A photo without a cavity number cannot guide a steel correction.

How Do You Turn Findings Into an Open-Issues List?

Write every finding down with its owner and its fix, and set a due date before you send anything back. Sort each finding into steel, process, design, or measurement. Steel means cutting or adding metal. Process means changing a setting on the sheet. Design means changing the part drawing, and that change needs your approval first.

Bundle the steel changes into one revision. Three separate requests over two weeks turn a short correction into a long one. Each request restarts scheduling, machining, trial time, and shipping.

Name the owner on your side and the owner on the supplier side for each item. A finding with no owner waits for the next trial to remind you it exists.

Send the list in writing, with the samples and the report attached. Verbal comments at a trial get lost between the press and the office. The written list is the scope for T2.

When Should You Approve, and When Should You Ask for T2?

Approve T1 only when the dimensions that decide fit meet the drawing. When a dimension misses, approve only with a written fix that names its owner and its date. Hold approval when a cavity runs out of tolerance with no known cause. Hold it when the process sheet is missing or lists machine settings only. A failed functional test blocks approval even when the dimensions read well.

Conditional approval works when the misses are small and the fixes are steel-safe. A steel-safe fix changes a dimension without moving a gate or a cooling line. Anything that moves those features needs a fresh trial before you sign.

Keep one approved sample as the golden sample, and mark it with the trial number and the date. Both sides keep a record of which sample was approved. The next trial is judged against that sample and the drawing together.

Your T1 Approval Checklist

Run this list before you sign, and hold the approval when any line fails.

  • Dimensions measured on parts from each cavity, kept separate by cavity.
  • Part weights recorded per cavity, with the gate-seal study attached.
  • Process sheet in plastic variables, with resin grade, lot, drying time, and mold temperature.
  • Fit and function tested on the assembled product, not on the part alone.
  • Defects photographed by cavity, each with a location and a cause.
  • Open-issues list in writing, each item with an owner, a fix, a due date, and a status.
  • Golden sample marked with the trial number and the date, and stored.

Sign only when every line above has evidence behind it, and send the T2 scope in the same message as the approval.